Question

Can you please tell me Std-OIT and HP-OIT for a pure unstabilized PP resin?

Answer

The HP-OIT test is preferred for long-term antioxidants that are sensitive to the high temperature of melting in the Std-OIT test. For unstabilized PP and PE, the situation does not arise and therefore the Std-OIT test should be adequate … Bob K.

Dr. Robert Koerner, GSI and GMA Techline

Join the discussion

To post a comment, visit: facebook.com/geosyntheticsmagazine or send your comments to editor Ron Bygness at rwbygness@ifai.com.

Comments and letters can contain opinions of individuals who are writing and do not necessarily reflect the views of Geosynthetics magazine or the Industrial Fabrics Association International.

Share this Story

Leave a Reply

Your email address will not be published. Required fields are marked *

Comments are moderated and will show up after being approved.